304 316 310S A36 Ss400 SPCC SGCC sovuq haddelenmiş/issiq prokatlangan zanglamaydigan po'latdan yasalgan plastinka

May 18, 2026 Xabar QOLDIRISH

Savol: SPCC ning odatiy tarkibi qanday?

A (wt%): C 0,12 dan kichik yoki teng, Mn 0,50 dan kichik yoki teng, P 0,035 dan kichik yoki teng, S 0,025 dan kichik yoki teng, Alt 0,020 dan katta yoki teng.

Savol: Yuqori va past uglerodli tarkibning ta'siri qanday?

Javob: Past C → yaxshi plastika, oson shtamplash, yaxshi payvandlanish qobiliyati; Yuqori C → kuch va qattiqlik, mo'rtlik ortdi.

Savol: SPCC past-uglerodli po'latmi?

Javob: Ha, C 0,12% dan kam yoki unga teng, odatda 0,05–0,10%.

Savol: SPCCda alyuminiyning roli qanday?

Javob: Deoksidlanish, donni tozalash, shtamplashning mustahkamligini oshirish va qarish mo'rtlashuvining oldini olish.

Savol: SPCC ning rentabellik kuchi qanday?

Javob: 140–280 MPa (odatda taxminan 210 MPa).